Antimicrobial, Bacterial Overgrowth, Dental White Spot, Evaluations, Diagnostic Self, Orthodontic Appliance Complication, Plaque, Dental, Plaque Induced Gingivitis
Conditions
Keywords
Nanoparticles, zinc oxide nanoparticle, coating, orthodontic molar tube, electrophoretic deposition cell, EPD CELL, nanomaterials, antimicrobial effect, bacterial culture
Brief summary
Orthodontic treatment is an elective procedure to improve the patient's dentofacial appearance. The complex design of fixed appliances provides a platform that leads to increased plaque accumulation around orthodontic brackets. So, the risk to develop demineralization area adjacent to orthodontic brackets is a major barrier in achieving this goal. Oral hygiene is greatly complicated following the placement of fixed orthodontic Appliances. Molar tube in place are considered for nearly all patients experiencing fixed orthodontic therapy over the whole treatment period, which normally lasts 1.5 to 2 years. To the best of the authors' knowledge, the application and antimicrobial efficacy of zinc oxide (ZnO) nanoparticles coating on orthodontic molar tube material has not been integrated clinically. White spot lesions during orthodontic treatment have a documented etiology. Briefly, the accumulation of plaque and food around brackets, bands, wires, and other attachments caused decreased pH and increased S. mutans colonization, which led to the possibility of clinical demineralization. The aims of study are to assess the antimicrobial effect of nanoparticle coated stainless steel orthodontic molar tube material (OMT) with zinc oxide (ZnO) nanoparticles in relative to uncoated orthodontic molar tube (UOMT) against the streptococcus. mutans& lactobacllius bacteria that cause white spot lesion around the fixed orthodontic appliance. .
Detailed description
Aim: The aim of this prospective randomized clinical trial is to assess the antimicrobial efficacy of nanoparticle coating stainless steel orthodontic molar tube (OMT) with zinc oxide (ZnO) nanoparticles in relative to uncoated orthodontic molar tube (UOMT). Objectives: 1. Compare the antimicrobial properties of the zno nanoparticle coated OMT in relative to uncoated orthodontic molar tube (UOMT). 2. Evaluate and compare the clinical bond failure rate between the coated OMT and the UOMT. The null hypothesis is that there is no significant difference in the antimicrobial effects and the rate of bond failure between the non-coated and coated stainless steel orthodontic molar tube using ZnO NPs.
Interventions
nine orthodontic patients each one will receive 2 coated zinc oxide nanoparticle molar tubes in split-mouth manner and will assess for antimicrobial effect on s. mutans & lactobacillus after two weeks, in addition to evaluation of bond failure rate after three months.
nine orthodontic patients each one will receive two uncoated molar tubes in split-mouth manner and will assess for antimicrobial effect on S. mutans & lactobacillus after two weeks, also, evaluation of the bond failure rate after three months period.
Sponsors
Study design
Masking description
When applications of orthodontic molar tubes to patients mouth through routine orthodontic treatment, the clinicians will explain the procedure to patients without knowing the about which side coated or not .
Intervention model description
72 orthodontic molar tubes will be divided in two groups control 36 uncoated OMT, and 36 experimental groups that will receiving the zinc oxide nanoparticle coating.
Eligibility
Inclusion criteria
* Patients who are seeking or under orthodontic treatment with fixed appliances Subjects must be healthy &well fit medically. * Subjects with no signs or symptoms of oral mucosal disease. * Subjects should not receive oral antimicrobials or antibiotic therapy for more than 3 months prior to sample enrolling. * non-pregnant or lactating Female patient. * Subjects is not smokers
Exclusion criteria
* Patients with a greater tendency to accumulate plaque (e.g., having congenital anomalies such as cleft lip and palate) or undergo orthognathic surgery
Design outcomes
Primary
| Measure | Time frame | Description |
|---|---|---|
| Evaluation of the antimicrobial Effect of ZnO Nanoparticles Coated orthodontic molar tube in relative to the uncoated orthodontic molar tube | After 2 weeks | Compare the antimicrobial properties of the zno nanoparticle coated OMT in relative to uncoated orthodontic molar tube (UOMT), through taking swaps from patient and sent to laboratory to culturing swaps samples to evaluating the colony forming unit number of S. mutans&lactobacillus bacteria which consider mean cause of white spot lesion and compare with the uncoated orthodontic molar tube swaps cultures. |
Secondary
| Measure | Time frame | Description |
|---|---|---|
| Evaluate and compare the clinical bond failure rate between the coated orthodontic molar tube and the uncoated orthodontic molar tube | 3 months | By following up patients for 3 months recording the bond failure occurs through out the this period with date and location of debond tubes for coated and uncoated orthodontic molar tubes. |
Countries
Iraq