Marginal Integrity of Hydroxyapatite Nanofiber Reinforced Flowable Composite
Conditions
Brief summary
This study will be conducted to evaluate the Marginal integrity of Hydroxyapatite Nanofiber reinforced flowable composite compared to a conventional resin-based flowable composite during management of initial carious lesion in adult population over a one year period.
Detailed description
A total of 26 volunteer patients with at least 2 non-cavitated molar teeth will be assigned in this study. Patients will be divided into two groups according to type of flowable composite (R) where groups R1 the pits and fissure will be sealed with Hydroxyapatite Nanofiber reinforced flowable composite while groups R2 the pits and fissure will be sealed with conventional resin-based flowable composite. Each restoration will be assessed after one week, six and twelve months Both materials will be applied according to manufacturer's instructions where teeth should be cleaned to remove surface stains, then select appropriate shade of the flowable composite, A rubber dam is the preferred method of isolation, etch and rinse adhesive system is applied, where acid etching will be applied for 15 seconds then rinse and dry followed by application of adhesive then light cure 10 seconds, then place and cure in 2 mm increments of the flowable composite for 20 s., gently remove oxygen inhibition layer after light cure with slurry of pumice or polishing paste All restorations were reviewed after 1 week, 6, 12 months by two investigators who were blinded to the material used for the restorations. All restorations were be evaluated by calibrated examiners following the FDI criteria
Interventions
assessment of marginal integrity of Conventional resin-based flowable composite
assessment of marginal integrity of Hydroxyapatite Nanofiber reinforced flowable composite
Sponsors
Study design
Eligibility
Inclusion criteria
* Patients should be over 18 Years old. * Patient should have good oral hygiene and general health * With at least 2 non-cavitated initial occlusal carious lesion first and/or Second molar teeth in each quadrant of maxilla or mandible
Exclusion criteria
* Known allergy to any of the resins used, * Clinically detectable caries, * Previously placed sealants or restorations, * Bruxism or malocclusion
Design outcomes
Primary
| Measure | Time frame | Description |
|---|---|---|
| marginal integrity of both restorations | 12 months | restorations will be reviewed after 12 months by two investigators who are blinded to the material used for the restorations. All restorations will be evaluated by calibrated examiners following the FDI criteria Data will be explored for normality using Kolmogrov-Smirnov test and Shapirowilk test. Comparisons between before and after treatment for normally distributed numeric variables will be done by Wilcoxon sign test. Comparisons between categorical variables will be performed using the chi square test Mcnemar test. A p-value less than or equal to 0.05 will be considered statistically significance. All tests will be two tailed. |