Dental defect
Conditions
Interventions
blank group 1:Following veneer preparation, the tooth surface is cleaned and air-dried. A 37% phosphoric acid gel is applied to the enamel surface for 20 seconds, then thoroughly rinsed and dried to a
0.5mm group:Bonding of 0.5 mm thick lithium disilicate glass ceramics on isolated teeth using 5 sets of energy laser treatments (140 mJ, 160 mJ, 180 mJ, 200 mJ, 220 mJ)
0.2mm group:Bonding of 0.2 mm thick lithium disilicate glass ceramics on isolated teeth using 5 sets of energy laser treatments (140 mJ, 160 mJ, 180 mJ, 200 mJ, 220 mJ)
blank group 2:enamel surface preparation
Sponsors
The Second Affiliated Hospital of Anhui Medical University
Eligibility
Sex/Gender
All
Age
20 Years to 50 Years
Inclusion criteria
Inclusion criteria: Diagnostic Criteria: Patients indicated for molar extraction. Inclusion Criteria: Intact crowns, without conditions such as dental caries, restorations, root canal treatments, or cracked teeth.
Exclusion criteria
Exclusion criteria: Extensive caries, tooth structure loss, cracked teeth, or root canal treated teeth.
Design outcomes
Primary
| Measure | Time frame |
|---|---|
| debonding time;Temperature changes in the pulp chamber;Tooth surface morphology;Veneer removal status;Veneer Fracture Patterns; | — |
Secondary
| Measure | Time frame |
|---|---|
| Veneer color and translucency evaluation;Veneer Mechanical Property Testing;Surface Roughness and Bacterial Adhesion Analysis of Veneers;Modifications of Adhesive Composition and Veneer Crystalline Structure; | — |